Founding - Abrasion resistant cast irons


Status:
Current
Type:
Standard
Language:
DA;EN
Price from:
€ 85.98

Scope

This European Standard defines the grades of abrasion resistant white cast irons. It specifies the grades in terms of:
- chemical composition;
- hardness.
The types of abrasion resistant white cast irons covered by this standard are:
a) unalloyed or low alloy cast irons;
b) nickel-chromium cast irons covering two general types:
- 4 % Ni 2 % Cr cast irons;
- 9 % Cr 5 % Ni cast irons;
c) high chromium cast irons covering four ranges of chromium content:
- 11 % < Cr </= 14 %;
- 14 % < Cr </= 18 %;
- 18 % < Cr </= 23 %;
- 23 % < Cr </= 30 %.
This European Standard does not define the abrasion resistant grades of ausferritic spheroidal graphite cast irons which are subject of EN 1564.


Number of pages: 44

Published: 2013-08-09

Date of approval: 2012-10-31

International relationships : EN 12513:2011 IDT

ICS: 77.080.10 - Irons